Why a single "particle size" is never enough
No real powder is made of identical particles. Even a carefully milled product contains a range, from a few fines to a few oversize pieces, with most of the material somewhere in between. Particle size distribution, or PSD, describes that whole range: how much of the material falls at each size.
This is why two lots with the same "average size" can behave completely differently. One might be a tight band of nearly uniform particles. The other might be a mix of dust and grit that happens to average out to the same number. The first flows and disperses predictably. The second segregates, dusts, and fails in the customer's process.
D10, D50, and D90 explained
Most PSD specs condense the distribution into a few percentile values, read off a cumulative curve:
D10: 10% of the material is smaller than this size. It describes the fine end.
D50: half the material is smaller and half is larger. This is the median particle size and the number most people quote.
D90: 90% of the material is smaller than this size. It describes the coarse end.
A powder reported as D10 = 4 µm, D50 = 12 µm, D90 = 30 µm tells you that the middle of the material sits around 12 microns, the finest tenth is under 4, and only a tenth is coarser than 30. Pigment, filler, and additive specs often add a D97 or D98, sometimes called the top cut, because a few coarse particles can cause streaks, specks, or nozzle clogs even when the median is perfect.
Span: how wide is the distribution?
The span compresses distribution width into one number:
Span = (D90 − D10) ÷ D50
Using the example above, (30 − 4) ÷ 12 gives a span of about 2.2. A smaller span means a tighter, more uniform product. Two lots with identical D50 values but spans of 1.0 and 3.0 are very different materials, and the span is often the more useful number for predicting flow, packing, and dispersion.
Reading a PSD curve
Lab reports usually show the distribution two ways. The cumulative curve is the S-shaped line that climbs from 0% to 100% as particle size increases; the D-values are read straight off it. The frequency curve (or histogram) shows how much material sits at each size, and is the easier one for spotting problems. A single smooth peak is typical of a well-controlled process. Two peaks, a bimodal distribution, usually means two populations: unmilled oversize mixed with milled product, fines generated by attrition, or two ingredients that were never fully reduced together.
Volume, mass, or number?
One detail trips up a lot of comparisons. A distribution can be weighted by volume, by mass, or by particle count, and the D50 changes depending on which one is used. Laser diffraction reports by volume. Sieve analysis reports by mass. Image analysis often counts particles. Because a single large particle carries as much volume as thousands of tiny ones, a number-weighted D50 can sit far below a volume-weighted D50 for the same powder. When a supplier's number does not match yours, check the basis before anything else.
How PSD is measured
Sieve analysis: shakes a weighed sample through a stack of screens and weighs what stays on each one. It is simple, durable, and widely understood, and it works best above about 38 to 45 microns. Our sieve analysis guide covers the method, and the mesh size chart translates screen numbers into microns.
Laser diffraction: measures how particles scatter a laser beam and calculates a volume distribution, covering sizes from well under a micron to a few millimeters. It is fast and repeatable, and it assumes spherical particles, which skews results for flakes and needles.
Dynamic image analysis: photographs particles as they pass a camera and measures each one, which also captures shape.
Sedimentation: infers size from how fast particles settle in a liquid. Still common for some fine minerals and pigments.
No method is "right" in the abstract. The best one is whichever matches how the spec was written and how the material will be used.
Changing a PSD in production
When a material does not meet its distribution spec, there are two basic moves. Size reduction pulls the whole curve to the left: jet milling and grinding reduce the D50 and D90, and jet milling can reach single-digit microns on many materials. Classification trims the ends of the curve: screening removes oversize or fines to tighten the span. Many projects use both, milling to get close and then screening to hit the top cut cleanly.
Frequently asked questions
What is particle size distribution?
Particle size distribution (PSD) describes the range of particle sizes in a powder and how much of the material falls at each size. It is usually reported as D10, D50, and D90 values or as a curve.
What does D50 mean?
D50 is the median particle size. Half of the material, by the stated weighting (usually volume or mass), is smaller than the D50 and half is larger.
What is the difference between D10, D50, and D90?
D10 is the size below which 10% of the material falls, D50 is the median, and D90 is the size below which 90% falls. Together they describe the fine end, middle, and coarse end of the distribution.
How do you calculate span?
Span equals D90 minus D10, divided by D50. A lower span means a narrower, more uniform particle size distribution.
Can a toll processor change my powder's particle size distribution?
Yes. Milling shifts the distribution finer and screening trims oversize or fines. US Chemical Services in Elyria, Ohio offers jet milling, grinding, and multi-deck screening with sieve testing; call (440) 529-8868.
Need help with your chemical processing project?